10.5281/zenodo.23235853Processed and derived data from an accelerated hygrothermal aging study of an epoxy barrier coating used for the rehabilitation of infrastructure. Coupons of a toughened epoxy composite were aged by dry-heat and by water immersion at four temperatures (20, 40, 60 and 80°C), for exposure periods ranging from an initial ~2-week sorption window to fourteen months of long-term gravimetric monitoring, and characterised by tensile testing (n = 5 specimens per condition), dynamic mechanical analysis (DMA; tan delta peak, ASTM D7028; n = 3 replicates) and differential scanning calorimetry (DSC; first heating scan; n = 3 replicates), together with gravimetric water-uptake measurements. This dataset contains the derived/processed results reported in the associated manuscript: tensile modulus, strength and elongation at break across four aging conditions — dry-heat aging for two months; water immersion for two months, tested wet; water immersion for two months followed by drying, to assess the reversibility of property loss; and water immersion for four months, tested wet — each reported across the four aging temperatures. Glass transition temperature (Tg) by DMA and DSC after two months of water exposure showed a comparatively narrow range (DMA ≈ 30–36°C; DSC ≈ 31–36°C) despite close to a two-order-of-magnitude change in tensile modulus over the same temperature range, indicating that Tg alone does not capture the extent of hygrothermal degradation in this system. Initial sorption rate constants at each temperature, together with an Arrhenius fit of the rate constant (apparent activation energy ≈ 10.1 kJ/mol, R² = 0.98, over 20–80°C), and the long-term (to fourteen months) 60°C weight-change curve are also included; the latter shows weight gain continuing for approximately eight months (peaking near 35%) before a subsequent decrease, consistent with a transition from diffusion-controlled moisture uptake to degradation-associated water transport (swelling, leaching, or partial network dissolution) at prolonged exposure. The raw, coupon-by-coupon water-uptake, mechanical and thermal data are openly available in DiVA and are not duplicated here; see Related works and References for the full set of underlying and related records.
Keyword(s):
accelerated aging; barrier coatings; dma; dsc; epoxy.
MeSH Term(s):
Grants and Funding:
No Grants or Funding Data Available
Associated Publication(s):
Supplementary Data:
No Supplementary Data Available
Related Dataset(s):
No Related Dataset Data Available
The National Library of Medicine (NLM) provides information about biomedical datasets. Inclusion on an NLM Web page does not imply endorsement of, or agreement with, the contents by NLM or the National Institutes of Health. Learn more: NLM Web Policies (nih.gov)