76vvhmstdtHand-crafted vibration features from five accelerated-life (run-to-fracture) tests of cracked 40Cr rotor shafts (Ø10 mm, 1000 r/min, fluctuating radial load 170–350 N, 12.8 kHz sampling). Each CSV has no header and 36 feature columns (3 channels × 12 features: vertical displacement, lateral displacement, axial acceleration). One row = one 1-s segment; 15 consecutive rows = one 15-s acquisition window; rows run in time order to fracture. R1/R3/R5 (shafts 10/40/60) are the training records and R2/R4 (shafts 20/50) the test records; R2 and R4 correspond to cracked rotors 4 and 5 in Khan et al., Measurement 239 (2025) 115433. These are the model inputs used in that paper and in the MF-GRU reproduction study. See README.txt for the file format, processing, labels and a note on the training records.
Keyword(s):
Accelerated Shelf Life; Crack; Remaining Useful Life.
MeSH Term(s):
Grants and Funding:
No Grants or Funding Data Available
Associated Publication(s):
No Associated Publication Data Available
Supplementary Data:
No Supplementary Data Available
Related Dataset(s):
No Related Dataset Data Available
The National Library of Medicine (NLM) provides information about biomedical datasets. Inclusion on an NLM Web page does not imply endorsement of, or agreement with, the contents by NLM or the National Institutes of Health. Learn more: NLM Web Policies (nih.gov)